Fine Silver Grain (99%)
Price:
$68.50
Product details
Description
99% pure silver in grain form. Guaranteed for purity and ethically sourced.
Casting and alloys Alloy composition, density, casting temperatures and a metal weight calculator.
Casting and Alloys Guide
Casting data for our gold casting alloys and silver casting grain, taken from each product's spec sheet: composition, density, hardness, melting and flask temperatures, plus a metal weight calculator.
Metal weight calculator
Weigh the wax model with its sprue, enter the weight in grams and pick the alloy and karat.
- Grams
- –
- Pennyweight
- –
- Troy oz
- –
Metal needed = wax weight × alloy density, plus 10% for the button.
Casting data by karat
| Alloy | Karat | Density (g/cm³) | As cast (HV) | Pre-alloying | Casting |
|---|---|---|---|---|---|
| 915 Premium White | 14K | 12.57 | 195 | 1060–1070 °C 1940–1958 °F |
1030–1050 °C 1886–1922 °F |
| 915 Premium White | 18K | 14.61 | 231 | 1060–1070 °C 1940–1958 °F |
1000–1025 °C 1832–1877 °F |
| 930 Ultra White | 10K | 10.99 | 164 | 1060–1080 °C 1940–1976 °F |
1055–1075 °C 1931–1967 °F |
| 930 Ultra White | 14K | 12.54 | 181 | 1050–1060 °C 1922–1940 °F |
1015–1035 °C 1859–1895 °F |
| 930 Ultra White | 18K | 14.58 | 226 | 1050–1060 °C 1922–1940 °F |
990–1010 °C 1814–1850 °F |
| 540 Premium Pink | 10K | 11.39 | 131 | 1050–1060 °C 1922–1940 °F |
1025–1045 °C 1877–1913 °F |
| 540 Premium Pink | 14K | 12.9 | 146 | 1050–1060 °C 1922–1940 °F |
990–1010 °C 1814–1850 °F |
| 220 Standard Yellow | 10K | 11.31 | 133 | 1010–1040 °C 1850–1904 °F |
975–995 °C 1787–1823 °F |
| 220 Standard Yellow | 14K | 12.83 | 135 | 1010–1040 °C 1850–1904 °F |
945–965 °C 1733–1769 °F |
| 230 Yellow, Extra Silver | 10K | 11.36 | 138 | 1010–1040 °C 1850–1904 °F |
960–980 °C 1760–1796 °F |
| 230 Yellow, Extra Silver | 14K | 12.87 | 148 | 1010–1040 °C 1850–1904 °F |
940–960 °C 1724–1760 °F |
| 315 Bright Yellow | 18K | 15.36 | 146 | 1030–1050 °C 1886–1922 °F |
975–995 °C 1787–1823 °F |
| Sterling silver grain | .925 | 10.22 | 78 | 1010–1040 °C 1850–1904 °F |
955–985 °C 1751–1805 °F |
| Anti-tarnish silver grain | .925 | 10.26 | 74 | 1010–1040 °C 1850–1904 °F |
960–990 °C 1760–1814 °F |
Full casting data, practice notes and hardening steps are in the guide. Open the full guide