JSP Gold Plus Dental Casting Alloy, item SA2015

JSP

JSP Gold Plus Dental Casting Alloy (50 g)

Price: $22.50

Part # SA2015

In stock

Same-day shipping is for approved trade accounts. Apply

Free shipping on orders over $200 and under 5 lbs. Add $177.50 more after this item.

$0 Free at $200
Weight 0.1 lb 5 lb limit

This item weighs 50 g.

Product details

Description

JSP Gold Plus is a copper-based, non-precious dental casting alloy with a yellow-gold color. It comes in a 50 g pack of ingots for professional dental laboratory casting. JSP describes it as a medium-fusing alloy with good flow and lists inlays, onlays, crowns, and bridges among its intended applications.

  • Pack size — 50 g of ingots
  • Melting range — 1,020–1,060 °C (1,868–1,940 °F)
  • Density — 7.8 g/cm³
  • Principal constituents reported by JSP — 80% copper, 7.8% aluminum, 3.5% iron, and 4.1% nickel
  • JSP part number — SA2015

Contains nickel. View JSP’s alloy specifications.

Casting and alloys Alloy composition, density, casting temperatures and a metal weight calculator.

Casting and Alloys Guide

Casting data for our gold casting alloys and silver casting grain, taken from each product's spec sheet: composition, density, hardness, melting and flask temperatures, plus a metal weight calculator.

Metal weight calculator

Weigh the wax model with its sprue, enter the weight in grams and pick the alloy and karat.

Grams
–
Pennyweight
–
Troy oz
–

Metal needed = wax weight × alloy density, plus 10% for the button.

Casting data by karat

Casting data by karat
Alloy Karat Density (g/cm³) As cast (HV) Pre-alloying Casting
915 Premium White 14K 12.57 195 1060–1070 °C
1940–1958 °F
1030–1050 °C
1886–1922 °F
915 Premium White 18K 14.61 231 1060–1070 °C
1940–1958 °F
1000–1025 °C
1832–1877 °F
930 Ultra White 10K 10.99 164 1060–1080 °C
1940–1976 °F
1055–1075 °C
1931–1967 °F
930 Ultra White 14K 12.54 181 1050–1060 °C
1922–1940 °F
1015–1035 °C
1859–1895 °F
930 Ultra White 18K 14.58 226 1050–1060 °C
1922–1940 °F
990–1010 °C
1814–1850 °F
540 Premium Pink 10K 11.39 131 1050–1060 °C
1922–1940 °F
1025–1045 °C
1877–1913 °F
540 Premium Pink 14K 12.9 146 1050–1060 °C
1922–1940 °F
990–1010 °C
1814–1850 °F
220 Standard Yellow 10K 11.31 133 1010–1040 °C
1850–1904 °F
975–995 °C
1787–1823 °F
220 Standard Yellow 14K 12.83 135 1010–1040 °C
1850–1904 °F
945–965 °C
1733–1769 °F
230 Yellow, Extra Silver 10K 11.36 138 1010–1040 °C
1850–1904 °F
960–980 °C
1760–1796 °F
230 Yellow, Extra Silver 14K 12.87 148 1010–1040 °C
1850–1904 °F
940–960 °C
1724–1760 °F
315 Bright Yellow 18K 15.36 146 1030–1050 °C
1886–1922 °F
975–995 °C
1787–1823 °F
Sterling silver grain .925 10.22 78 1010–1040 °C
1850–1904 °F
955–985 °C
1751–1805 °F
Anti-tarnish silver grain .925 10.26 74 1010–1040 °C
1850–1904 °F
960–990 °C
1760–1814 °F

Full casting data, practice notes and hardening steps are in the guide. Open the full guide